The crack is not a screed failure. It is a missing
detail.
A heated screed is a slab that changes size. It is warmed, it expands; it
cools, it contracts. Around its perimeter it is held by walls, columns and
thresholds — and wherever it is held, the movement it cannot release outward it
releases somewhere else, usually as a crack.
The crack is then read as a material fault, a mixing fault, or a "bad
batch". Almost always it is none of those. It is the predictable result of
casting a moving slab as though it were a static one.
What actually moves
Two things move, and only one of them matters much:
The pipe expands and contracts, but it is fully embedded and restrained by
the screed around it. Its movement is absorbed by the surrounding material and
by its own flexibility. This is why flexible pipe is specified in the first
place.
The screed expands and contracts as a slab, and it is far stiffer than the
pipe. This is the movement that produces cracks, lifting at thresholds and tile
debonding.
The practical consequence: detail for the slab, not for the pipe.
Where cracks appear, in order of frequency
1.Doorways. A doorway is a narrow neck between two large areas. Movement
from both sides concentrates there.
2.Long corridors and narrow strips. Same mechanism, at a smaller scale.
3.Internal corners and re-entrant angles. Stress concentrates at the change
of geometry.
4.Where the screed abuts rigid elements — columns, stair cores, steel
stanchions.
5.Along the boundary of an unheated area — a step in temperature across a
short distance.
If a crack has appeared in a heated floor, the first question is not "what
was wrong with the mix" but "where was the nearest movement joint".
The joints that prevent it
Perimeter joint. A compressible strip fixed to every wall and every rigid
element before the screed is placed. The screed is then free to move at its
edges. Tucking screed tight to a wall is the single most common omission on
site, and it converts a perimeter into a restraint.
Bay joints. Large areas are divided so that movement in each bay stays
manageable. Spacing follows the screed specification and the applicable standard
— it is not a rule of thumb to be decided on site.
Joints at doorways and at changes of section. A doorway should be treated
as a joint location, not as a place to run the screed through continuously
because it looks tidier.
Joints must be carried through the finish. This is where a correct screed
detail is undone: a movement joint in the screed with a continuous, rigidly
bonded tile bed over the top simply transfers the crack up into the tiling, in a
straight line, months later. The joint has to continue through the tile bed, or
the covering has to be able to accommodate the movement.
The pipe where it crosses a joint
A loop crossing a movement joint needs protection: a short sleeve or a
length of conduit over the pipe at the crossing, so that movement of the slab
does not shear or abrade the pipe.
This is a small detail with a large consequence. A pipe pinched at a joint
is a future leak in a place nobody will look.
First heat-up is part of the detail
The screed has to be brought up to temperature gradually, and the rate
belongs to the screed supplier and the applicable standard rather than to the
installer's judgement. Heating a new screed hard and fast is a common cause of
cracking that later gets blamed on the mix.
The pipe will tolerate it. The screed will not.
Reading a crack correctly

Checklist before the pour
1.Compressible strip on every wall and every rigid element — continuous,
not butted in pieces.
2.Joint positions agreed and marked: doorways, changes of section, bay
boundaries.
3.Pipe sleeved at every joint crossing.
4.Pipe pressurised and recorded during the pour, so a damaged loop is found
the same day.
5.Cover depth over the pipe as specified — no thin spots at high
points.
6.Heat-up procedure agreed in writing with the screed supplier, and
scheduled.
A heated floor is a moving assembly. RITABLE supplies the underfloor
heating components — pipe, manifolds and bend supports — that make the detailing
practical on site.